| PRODUCTS |
FUNCTION |
APPLICATION |
| CRAFTCOTE-CEN |
Insulating coating |
CRAFTCOTE – CEN is recommended for all C.I. Casting. It can be applied by dipping / brushing application. Thick coating to be applied to get good insulating effect. The insulating property of coating reduces the solidification rate of metal. Recommended for reducing the chilling / hardening of metal at thin wall section casting.
After applying coating air dry it for 10 to 20 minutes and then dry in oven at 150°C to
160 °C for min. 20 minutes or by torching.To insure moisture free. |
| CRAFTCOTE-CEN(M) |
Centrifugal dicasting coating |
Ensure that die is free from foreign material and dust. Stir the coating and dilute it by ratio 100:5 to 100:10 ( i.e. product : water). Apply by spraying on hot die (at die temperature 150° C to 180° C) and coat up to 1mm thickness. If thickness is not achieved in one spray, apply again. Keep the die rotating while spraying CRAFTCOTE – CEN (M), so as to get uniform coating thickness. Now pour the metal.
After removing casting, again clean the die surface and apply coating by
same procedure. |
| CRAFTCOTE-SN |
Special Inoculation Coating |
Apply CRAFTCTOE - SN as it is on sand mould/core by brushing. If the permeability of sand is more then we recommend to have a precoat with zircon or other mixed refractory water based coating. Dry the coating and then apply CRAFTCOTE- SN. Dry it in oven at 120° C for 1 hr. Ensuring removal of moisture from the coating. Mould/ Core is then ready for pouring. Do not apply other coating on CRAFTCOTE- SN. |
| CRAFTCOTE-TE |
SPECIAL CHILLING COAT |
- CRAFTCOTE - TE is to be applied as it is by brushing or swabbing after uniform
mixing. If required coating can be further diluted with water in case thinner coating
consistency is needed.
- Mould or core should be thoroughly dried before pouring the metal. (Do not heavily
torch the coating) .
- Whenever double coating is required take care that the previous coat is thoroughly
air dried.
|
| CRAFTCOTE-TES |
CHILLING COAT |
- CRAFTCOTE – TES is to be applied as it is by brushing or swabbing after uniform mixing.
- Mould or core should be thoroughly dried before pouring the metal. (Do not heavily torch the coating).
- Whenever double coating is required take care that the previous coat is thoroughly
air dried.
- For economical practice, give first coat of zircon base coating on the portion when CRAFTCOTE – TES is to be used.
|