CERAFLUX GR-510W

Granulated Medium To Low Exothermic Drossing Flux For Aluminium And Aluminium Alloys

Product

CERAFLUX GR-510W is a flux with a moderately high temp. reacting. Suitable for al sodium tolerant Aluminium Alloys.

CERAFLUX GR-510W is most suited for use in the central melting furnaces, chip melting and transport ladles and will aid in keeping furnace walls free of corundum build-up.

Purpose

CERAFLUX GR-510W can be used on moderately high metal temperatures in sand, die and High pressure die casting foundries. It produces dry ash-like dross that is easily separated from the molten metal. Skimming is thus facilitated and metal loss due to aluminium entrapment in the dross is reduced.

CERAFLUX GR-510W is scattered on the surface of the molten metal or can be applied by using flux injection machine at a rate of 0.05 - 0.15% of the metal weight. The flux is then rabbled gently into the melt until the exothermic reaction develops. The powdery dross is either pushed aside or preferably removed before taking the ladles of metal for die casting.

Application Temperature: 670-750°C

Benefits

CERAFLUX GR-510W specially developed to be environmentally friendly. It is dust free in use and emits low fume during application.

  • Granulated fluxes can be used at reduced application rates compared to powder fluxes.
  • Granular ensuring uniform chemical composition through-out flux.
  • 2-4 mm designed for flux injection machine.

Standard Packing : 20 kg polyethylene lined paper sacks

Precaution : Flux Is Hygroscopic In Nature So Store It In Dry Atmosphere.

Material Safety Data Sheet (MSDS) is Available on Request

Our Products

We offer a wide range of foundry products and services to meet the requirements of iron, steel and non-ferrous
foundries to help them to reduce defects, improve casting quality and optimise production costs.